Rubber roller covering tape for textile industry

Rubber roller covering tape for textile industry is a kind of widely used rubber cloth products developed and produced by our company in recent years by taking advantage of our equipment. Rough belt is also known as rough rubber (wrapped roller belt, rough rubber, prickly skin, granular rubber, granular rubber, wrapped roller skin, roller wrapped skin, granular belt, granular skin, granular belt, granular skin, rough skin, roller skin, anti-slip belt). Rough surface belt is used to increase the coefficient of friction and is usually used for fabric traction in different processes in the textile industry, such as being used on the guide rolls of various air-jet, water-jet, rapier, piece-shuttle and other shuttle-less looms as well as fabric checking and dyeing equipments.

Application Scenarios

  • Model Parameters Table

    ModelThicknesses(mm)Temperature resistance(℃)

    Effective pulling force

    (N/mm)

    MatterGrain Color

    KQ0901

    KQ0902

    KQ0903

    KQ0904

    KQ0905



    1.8~2.0



    -10~110



    35



    NBR/polyester fabric



    rough surface

    gray

    white

    yellow

    blue

    red

    KQ0911

    KQ0912

    1.8~2.0-10~11035NBR/polyester fabriccoarsely woven fabric pattern

    gray

    white

    KQ0921

    KQ0922

    1.8~2.0-10~11035NBR/polyester fabricpinstripe

    gray

    white

    KQ09311.8~2.0-10~11035NBR/polyester fabricmatte finishgray
    KQ09411.8~2.0-10~11035NBR/polyester fabricglossy sidepink
    KQ09511.8~2.0-10~11035NBR/polyester fabricround granular surfaceblue