Model | Tensile strength(Mpa) | Tear strength(N/mm) | Hardness (Shore A) | Elongation at break (%) | Color | Surface detail |
KQ3111 | 6.5 | 26 | 55±5 | 450 | Transparent | Smooth on both sides |
KQ3112 | 6.5 | 26 | 55±5 | 450 | Transparent | Smooth on one side and patterned on the other |
KQ3121 | 6.5 | 26 | 55±5 | 450 | Rust red | Smooth on both sides |
KQ3122 | 6.5 | 26 | 55±5 | 450 | Rust red | Smooth on one side and patterned on the other |
KQ3211 | 8.0 | 32 | 55±5 | 650 | Transparent | Smooth on both sides |
KQ3212 | 8.0 | 32 | 55±5 | 650 | Transparent | Smooth on one side and patterned on the other |
KQ3221 | 8.0 | 32 | 55±5 | 650 | Rust red | Smooth on both sides |
KQ3222 | 8.0 | 32 | 55±5 | 650 | Rust red | Smooth on one side and patterned on the other |