Glass silicone sheet (full name: Silicone Sheet for Vacuum Bag of Glass Laminating Furnace): The vacuum bag composed of silicone sheet is used in the glass laminating furnace to thermally bond the glass and EVA film (also known as EN film) together under the condition of vacuum while heating, i.e., to form the safety laminated glass. Vacuum bag is the core component of glass laminating furnace, which is composed of upper and lower two silicone sheets and shaped silicone sealing strips. The silicone sheet is the key component of the whole laminating furnace, and its quality directly affects the quality of glass products.

Application Scenarios

  • Model Parameters Table

    Model

    Tensile strength(Mpa)

    Tear strength(N/mm)

    Hardness (Shore A)

    Elongation at break (%)

    Color

    Surface detail

    KQ3111

    6.5

    26

    55±5

    450

    Transparent

    Smooth on both sides

    KQ3112

    6.5

    26

    55±5

    450

    Transparent

    Smooth on one side and patterned on the other

    KQ3121

    6.5

    26

    55±5

    450

    Rust red

    Smooth on both sides

    KQ3122

    6.5

    26

    55±5

    450

    Rust red

    Smooth on one side and patterned on the other

    KQ3211

    8.0

    32

    55±5

    650

    Transparent

    Smooth on both sides

    KQ3212

    8.0

    32

    55±5

    650

    Transparent

    Smooth on one side and patterned on the other

    KQ3221

    8.0

    32

    55±5

    650

    Rust red

    Smooth on both sides

    KQ3222

    8.0

    32

    55±5

    650

    Rust red

    Smooth on one side and patterned on the other